Lamination Peeling off after 2 to 3 months

$
0
0
Hi,

We are using Thermal Lamination on our sheet fed printing sheets. Recently we observed lamination is peeling of after 2 to 3 months period. We use films 20 to 30 microns range always & we keep thermal cylinder temperature around 100 to 120 degrees Celsius.

I would like to know how to adjust temperature and Nip pressure according microns of the film, Gloss & Matt types. We generally keep littler higher temperature for Matt films.

How to adjust if paper GSM is vary.